<?xml version="1.0" encoding="UTF-8"?><?xml-stylesheet type="text/xsl" href="static/style.xsl"?><OAI-PMH xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/ http://www.openarchives.org/OAI/2.0/OAI-PMH.xsd"><responseDate>2026-06-07T15:18:36Z</responseDate><request verb="GetRecord" identifier="oai:docta.ucm.es:20.500.14352/60380" metadataPrefix="mods">https://docta.ucm.es/rest/oai/request</request><GetRecord><record><header><identifier>oai:docta.ucm.es:20.500.14352/60380</identifier><datestamp>2024-10-29T14:04:07Z</datestamp><setSpec>com_20.500.14352_14</setSpec><setSpec>col_20.500.14352_15</setSpec></header><metadata><mods:mods xmlns:mods="http://www.loc.gov/mods/v3" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xmlns:doc="http://www.lyncode.com/xoai" xsi:schemaLocation="http://www.loc.gov/mods/v3 http://www.loc.gov/standards/mods/v3/mods-3-1.xsd">
   <mods:name>
      <mods:namePart>Del Nero Beneitez, María Olga</mods:namePart>
   </mods:name>
   <mods:name>
      <mods:namePart>Macorra García, José Carlos De La</mods:namePart>
   </mods:name>
   <mods:extension>
      <mods:dateAvailable encoding="iso8601">2023-06-20T20:30:38Z</mods:dateAvailable>
   </mods:extension>
   <mods:extension>
      <mods:dateAccessioned encoding="iso8601">2023-06-20T20:30:38Z</mods:dateAccessioned>
   </mods:extension>
   <mods:originInfo>
      <mods:dateIssued encoding="iso8601">1999</mods:dateIssued>
   </mods:originInfo>
   <mods:identifier type="issn">0361-7734</mods:identifier>
   <mods:identifier type="uri">https://hdl.handle.net/20.500.14352/60380</mods:identifier>
   <mods:abstract>The objectives of this research were (1) to analyze the variations of the permeability of dentin after restoration with two polyacid-modified resin composites (Compoglass, Dyract) and four single-bottle adhesives (Prime &amp; BOnd 2.0, Syntac Single Component, OptiBond Solo, and Single Bond -Scotch Bond 1 in Europe- immediately (approximately 1 hour) after insertion. A perfusion system with distilled water was used at a pressure of 32.5 cm of water; (2) to study the bond strength of their interfaces; and (3) to find the correlation, if any, between both parameters. None of the materials used produces a complete cessation in fluid filtration. Tensile strengths were very low (maximum: P&amp;B=3.96MPa) probably because of the very large bonding surfaces used (mean bonded surface area = 88.8mm²). No significant correlation was found between tensile bond strength and the sealing ability for any material.</mods:abstract>
   <mods:language>
      <mods:languageTerm>spa</mods:languageTerm>
   </mods:language>
   <mods:accessCondition type="useAndReproduction">open access</mods:accessCondition>
   <mods:titleInfo>
      <mods:title>Sealing and Dentin Bond Strengths of Adhesive Systems</mods:title>