Method to compare [mu]-tensile bond strength of a self-etching adhesive and [mu]-cohesive strength of adjacent dentin
dc.contributor.author | Macorra García, José Carlos De La | |
dc.contributor.author | San Nicolás, Adriana | |
dc.date.accessioned | 2023-06-20T12:41:48Z | |
dc.date.available | 2023-06-20T12:41:48Z | |
dc.date.issued | 2005-10 | |
dc.description.abstract | Laboratory results from tensile or micro-tensile testing of adhesive/restorative systems need a gold standard to make their interpretation possible. This can be done by comparing the [mu]-tensile bond strength ([mu]TBS) of the tested adhesive(s) with the [mu]-tensile cohesive strength ([mu]TCS) of the adjancent dentin, which in meant to be replaced by the restoration. Objectives: to test immediate [mu]TBS of and adhesive/restorative system versus [mu]TCS of the dentin adjacent to the bonded interface, in perfused specimens. Methods: enamel and roots of five-third sound molars were removed and teeth were perfused (30 cm distelled water) until after the bonding procedure was completed. Parallel grooves (1.5-mm wide X 1.5-mm deep, separeted by 1.5 mm), were drilled in the exposed dentin, under water refrigaration. Teeth were restored (AdheSE/Filtek Z250). Specimens were sawn from grooves to test [mu]TBS (n=32) of dentin, adjacent to adhesive interfaces, both areas to be tested at the same relative depth. Areas to be studied were rounded (mean bonded surface area for both groups, BA=0.68 mm2), and [mu]TBS and [mu]TCS were found. As not all BAs were identical, residuals of [mu]TBS and [mu]TCS values to the regression line relating BA and tensile test result (representing the null hypothesis, i.e. [mu]TBS=[mu]TCS) were compared using a non-parametric test. Results: difference in the means of residuals was not stadistically significant (two tails p=0.067). Significance: mean [mu]TBS of the tested adhesive was nor different to mean [mu]TCS of adjacent dentine. The null hypothesis was not rejected. | en |
dc.description.department | Depto. de Odontología Conservadora y Prótesis | |
dc.description.faculty | Fac. de Odontología | |
dc.description.refereed | TRUE | |
dc.description.status | pub | |
dc.eprint.id | https://eprints.ucm.es/id/eprint/5048 | |
dc.identifier.citation | Delamacorra J, Sannicolas A. Method to compare μ-tensile bond strength of a self-etching adhesive and μ-cohesive strength of adjacent dentin. Dental Materials 2005;21:946–53. https://doi.org/10.1016/j.dental.2004.11.007. | |
dc.identifier.doi | 10.1016/j.dental.2004.11.007 | |
dc.identifier.issn | 0109-5641 | |
dc.identifier.officialurl | https//doi.org/10.1016/j.dental.2004.11.007 | |
dc.identifier.relatedurl | http://www.sciencedirect.com/science?_ob=MImg&_imagekey=B6VP3-4G3SC8T-3-7&_cdi=6195&_user=144492&_orig=browse&_coverDate=10%2F31%2F2005&_sk=999789989&view=c&wchp=dGLbVlz-zSkWW&md5=eea6a773d38969ebe0a9e697f5a6a960&ie=/sdarticle.pdf | |
dc.identifier.uri | https://hdl.handle.net/20.500.14352/52252 | |
dc.issue.number | 10 | |
dc.journal.title | Dental materials | |
dc.language.iso | spa | |
dc.page.final | 953 | |
dc.page.initial | 946 | |
dc.rights.accessRights | open access | |
dc.subject.keyword | Micro-tensile bond strength | |
dc.subject.keyword | Micro-cohesive dentin strength | |
dc.subject.keyword | Self-etch adhesive | |
dc.subject.keyword | Dentin | |
dc.subject.ucm | Odontología preventiva | |
dc.subject.ucm | Materiales dentales | |
dc.subject.unesco | 3213.13 Ortodoncia-Estomatología | |
dc.title | Method to compare [mu]-tensile bond strength of a self-etching adhesive and [mu]-cohesive strength of adjacent dentin | en |
dc.type | journal article | |
dc.volume.number | 21 | |
dspace.entity.type | Publication | |
relation.isAuthorOfPublication | 0b38ba8d-c9aa-404d-8ec6-b8c2d6a78884 | |
relation.isAuthorOfPublication.latestForDiscovery | 0b38ba8d-c9aa-404d-8ec6-b8c2d6a78884 |
Download
Original bundle
1 - 1 of 1
Loading...
- Name:
- Method_to_compare_u-tensile_bond_strength_of_a_self-etching.pdf
- Size:
- 220.37 KB
- Format:
- Adobe Portable Document Format